Celanese VAM HQ 8-10
Home Standard VAM Celanese VAM HQ 8-10

Celanese VAM HQ 8-10

Vinyl Acetate Monomer HQ 8-10 · inhibitor 8-10 ppm

Celanese VAM HQ 8-10 product packaging
Standard VAM

Vinyl Acetate Monomer HQ 8-10

For polyvinyl butyral and interlayer work, where the usual source of an off-spec batch is moisture rather than inhibitor level. The band carries a plant through a normal delivery cycle, and the grade is normally specified together with a water limit that the receiving team is expected to protect rather than test for after the fact.

HQ 8-10 ppmMoisture controlPVB and interlayers

Request a quotation

Typical properties

Specification Snapshot

Typical values, not for specification. Batch certificate governs delivery.

Chemical nameVinyl Acetate Monomer (VAM)
CAS / EINECS108-05-4 / 203-545-4
Formula / MWC4H6O2 / 86.09
AppearanceClear, colourless liquid, free of suspended matter
VA purity≥ 99.9 wt% (typical)
Water≤ 200 ppm (0.02 wt%, typical)
Acidity as acetic acid≤ 50 ppm (typical)
Acetaldehyde≤ 50 ppm (typical)
Methyl acetate≤ 50 ppm (typical)
Ethyl acetate≤ 250 ppm (typical)
Colour≤ 5 Pt-Co (typical)
Distillation range @760 mmHg72.3 – 73.1 °C
Density @20/20 °C0.9320 – 0.9345 g/cm³
Boiling point72.7 °C
Melting point− 93.2 °C
Flash point (closed cup)− 8 °C
Autoignition temperature385 – 427 °C (source dependent)
Explosive limits in air2.6 – 13.4 vol%
Vapour pressure @20 °C11.7 kPa
Vapour density (air = 1)3.0
Solubility in water @20 °C≈ 2 g/100 mL
Refractive index n20/D1.395
Inhibitor (hydroquinone, HQ)8-10 ppm
Storage stabilityDepends on temperature, oxygen availability and inhibitor consumption; periodic HQ and polymer re-test recommended
Humidity and moisture ingress

Humidity and Moisture

In a coastal plant the tank breathes every day, and each breath carries water. This section covers the practical defences and the checks that show whether they are still working.

A storage tank is not sealed. As the shell warms and cools the headspace expands and contracts, and every inward breath brings ambient air with its humidity. In a dry inland site this is a slow effect; in a coastal plant with a wide day-night swing it can move the water figure within a week. That is why the drying arrangement deserves the same attention as the inhibitor test.

The response is a combination rather than a single device. A desiccant on the vent, a slight positive pressure and a predictable fill-and-draw pattern all reduce the volume of moist air reaching the product. The check is not whether the desiccant is present but whether it is still active: a spent cartridge looks like a working one, and only a scheduled change with a written date distinguishes them.

  • Confirm vent drying is fitted and dated
  • Keep a slight positive pressure where allowed
  • Test water at the tank outlet, not the top
  • Close drums the same shift they are opened
Handling

Processing Notes

Stainless steel or aluminium only. Confirm the headspace practice against documented supplier guidance instead of assuming a nitrogen blanket is protective.

Water specification

Treat the water limit as a receiving control, not a laboratory formality. A routine check at intake catches a desiccant failure before the material reaches an interlayer batch.

Drum handling

Where drums are used for small additions, open them in a dry area and close them the same shift. A part-used drum in a humid store is the most common route for water to enter an otherwise well-run plant.

Tank breathing

Consider a dry-air pad or a desiccant vent rather than an open vent on coastal sites, and shade the shell to reduce the daily breathing cycle that drives the whole problem.

Analytical routine

Measure water with a method suited to the low levels involved and keep the trend. A single passing result says little; a rising line tells you the drying arrangement has stopped working.

Applications

Where It Fits

Each route below links to the application map for the full grade set.

Interlayer resins sensitive to water content

Coastal binder plants with humid storage

Emulsion lines demanding a dry feed

Coating kitchens in humid climates

Delivery

Packing and Delivery

Every export lot ships with a batch certificate of analysis.

Bulk
ISO tank with dried vent
Packed
200 L steel drums, sealed
Documents
Batch analysis per lot
Cross reference

Related Grades

Compare the inhibitor band, storage window and delivery form side by side.

Knowledge base

Related News

Technical, knowledge and commercial notes written for this product line.

All news

Contact

Request a Quotation

Send your required volume, delivery form and site for Celanese VAM HQ 8-10; we reply with the matching grade, the batch documentation and the shipping window.

WhatsApp QR code for Fred Wang
Fred Wang
Scan to WhatsApp — +8615380400285
sales2@liwei-chem.com